Casting Lead Sling Bullets (Read 1943 times)
Matthew Skinner
Guest


Casting Lead Sling Bullets
Apr 6th, 2005 at 3:17am
 
Have recently started looking at Slinging as a hobby, and being from a country where there's lots of out door and as someone who likes the traditional way of doing things. I thought I'd try out making my own lead bullets. (Already braided my own sling) I noticed alot of the advice offered didn't cover how casting was done in detail apart from the the Romans did thier casting in sand. (That and the modern versions which I am not interested, sorry guys.)

Anyway after much though, net surfing, asking nerdy friends, and general stubourness. I found out two things of interest to those who would like to make thier own.

Sand Casting is done with a mixture of sand, water and 11%-30% clay. This is usually fire clay. 

More info:
http://www3.telus.net/public/aschoepp/sand.html

That done I then looked into how lead casting is done which was very interesting. (If your me I suppose)  I was wondering if anyone here as actual cast thier own bullets in a traditional method and if they had any pointers before I go and mess up my first batch as per usual. 

Onto my next bit. Sand casting is done in two halves. (Like we didn't already know) What I found interesting was that before the  casting there is usually a empty space, for want of a better word, which holds the excess metal. I hazard a guess that this is to keep pressure on the casting, but I could be wrong; This leads me to my next question does anyone know why and do they do it?

Well that's it I'll post if all goes well, or not.
Back to top
 
 
IP Logged
 
Zorrro
Funditor
****
Offline


Yeah, i guess most of
us love YaBB 1G - SP1!

Posts: 530
Granada (Spain)
Gender: male
Re: Casting Lead Sling Bullets
Reply #1 - Apr 6th, 2005 at 8:08am
 
Hi Matt i've done some casting "the old way"  .45 lead balls for my slingshot...  my  cast was entirely made of red clay, i modelled a cube, splitted in two halves witha piece of thread, stabbed a lead ball .45 on one half fresh clay cast deep to the ball equator. Then i pressed the other fresh clay half cast to cover all the lead ball.
Then separate the two halves take away the lead ball and let dry completly.
Next fire the clay (i did it in an electric cook oven) Once the cast has been fired  iscrapped a funnel-like entrance on the two halves of the cast with a file to allow melted lead to fill the spheric hollow. (i had to resize this funnel a bit bigger cause at first lead didn't passed trough).
For casting the lead balls i hold together the two halves of the cast with pliers, and pour the lead inside (funnel-like hole on the upper side)
Usually the 1st and may be 2nd balls were not good cause clay cast  was cold, but when it got hot, lead balls were nice solid.  The clay cast gets a lot hot, and keep hot for long, so you have to handle it with pliers.
Part of the funnel-like hole gets fill with the lead. Maybe that's what you noticed as ----------"What I found interesting was that before the  casting there is usually a empty space, for want of a better word, which holds the excess metal. I hazard a guess that this is to keep pressure on the casting,"---------  just cut out this excess of lead with the pliers or scissors. Also there's an equatorial mark of the two halves of the cast, but this won't be a problem for a slingshot or a sling. you can sand or file it if you don't like how it looks Smiley
Clay reduce it's size when gets dry, so balls were sightly under .45  anyway a slingshot or a sling can deal ok with the difference Smiley May be a mix of sand and clay is better to work with, and doesn't reduce it's size as much as clay alone.
Back to top
 

Never disturb your enemy when it's making a mistake (Napoleon Bonaparte)
 
IP Logged
 
Matthias
Past Moderator
*
Offline



Posts: 1418
Gatineau/Ottawa QC, Canada
Gender: male
Re: Casting Lead Sling Bullets
Reply #2 - Apr 6th, 2005 at 1:29pm
 
The resevoir(s) are often called risers, and are placed so that they can feed excess metal back into the mold as the casting cools to avoid defects caused by shrinkage. Metals expand a lot when they are molten, and if no allowances are made you don't get smooth/strong results.

Normally, the risers are connected to any point in the casting that will be the hottest, or cool the most slowly. Luckily, for simple shapes like glandes, you can usually rely on the sprue (where you pour the lead) providing enough "spare" metal. As the shapes get more complicated you need more and more tricks (a whole distribution/venting/temp control network!) to ensure good results.

Matthias
Back to top
 
 
IP Logged
 
Douglas_The_Black
Interfector Viris Spurii
*****
Offline


Hakkaa päälle!

Posts: 3491
Salineville Ohio
Gender: male
Re: Casting Lead Sling Bullets
Reply #3 - Apr 6th, 2005 at 8:56pm
 
haha interesting to you? trust me any thing to do with the sling we are usaly quite interested in.  Smiley


Im a big fan of the "lost wax" method that sounds alot like what you are doing. I just dig up some clay, get some bees wax or candel wax melt the stuff down and shape it.

then i cover it up with a generous portion of clay, leaving a hole up top, let the stuff set out in the sun for a few days then i just toss it into the fire pit after im done having my hot dogs. Cover the whole thing up with hot coals and let it set in the hot coals for a few hours. i like to let it set for a day. Pull the mold out melt your lead, heat your mold back up then poor the lead in.

after a while you just throw the clay mold down shattering it and you pick up your nice gland.


also i like to just make clay shots. all you have to do is get some clay and mold it into the shape you like. and do the fire method described above.

some tips of using clay

first of all if your digging it up i like to let it dry, then grinde it up into a powder, then pick out all of the rocks. getting the dirt out is much harder to do and i havent as of yet figured it out. but once you have your powderd clay just add a little water and it works fine.

that book we where talking about in the other topick if i where to write a chapter for that book (indeed i would love to) i would do it on clay. its about the best thing i am good at.  Smiley
Back to top
 

i live in a maze of typo's&&&& popularity is for dolls a hero cannot be popular-Ralph Waldo Emerson&&&&DTB-master of the corny vest, and crappy carpet!